Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.0 GPa | 2180 ksi | ASTM D638 |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | |
LATI Latiohm 66-07 PD08 G/30 PA66, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9290 PET (Europe-Africa-Middle East) 45% GF PET, Glass, Mold Release, Heat Stabilized, |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific) LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | |
Cytec Thornel® VCK Carbon Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | |
Cytec Thornel® VCL Carbon Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527-1/-2 |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4217 black 9233 PA6T/66-GF45 Product description: Grivory XE 4217 black 9233 is a high heat stabilized, 45% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection moulding. Polymer designation.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527-1 |
Barlog Plastics KEBAFLOW HF140 LCP, 40% glass fiber reinforced LCP-GF40Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527-1 |
Barlog Plastics KEBATER BF250 PBT, 50% glass fiber reinforced, food grade PBT-GF50Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Conditioned, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 15.0 GPa @Temperature 70.0 °C, Time 180000 sec |
2180 ksi @Temperature 158 °F, Time 50.0 hour |
62% RH |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 1mm/min; ISO 527 |
BASF Ultramid® B3EG10 BK00564 50% Glass Filled PA6 (Dry) Ultramid B3EG10 BK00564 is a 50% glass fiber reinforced injection molding PA6 grade. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Vyncolit X611 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6, FR, compliant with ECO protocols, non-brominated, non-chlorinated |