Mechanical Properties Metric English Comments
Tensile Modulus 152 GPa
22000 ksi
PSM Industries Pacific Sintered Metals 4600 F-253-T(HT) Powdered Metal
High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-140HTInformation Provided by Pacific Sintered Metals, a division of PSM ..
Tensile Modulus 152 GPa
22000 ksi
0°; ASTM D3039
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg
Arovex® 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (121°..
Tensile Modulus 152 GPa
22000 ksi
Typical epoxy composite property
Hexcel® HexTow™ AS7 Carbon Fiber
HexTow™ AS7 carbon fiber is a continuous, high strength, high strain, PAN based fiber available, in a 12,000 (12K) filament count tow. This fiber has been surface treated and can be sized to improv..
Tensile Modulus 152 GPa
22000 ksi
Eagle Brass 715 Copper Nickel 30%, 1/2 Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Modulus 152 GPa
22000 ksi
Eagle Brass 715 Copper Nickel 30%, 1/4 Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Modulus 152 GPa
22000 ksi
Eagle Brass 715 Copper Nickel 30%, Annealed
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Modulus 152 GPa
22000 ksi
Eagle Brass 715 Copper Nickel 30%, Extra Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Modulus 152 GPa
22000 ksi
Eagle Brass 715 Copper Nickel 30%, Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Modulus 152 GPa
22000 ksi
Eagle Brass 715 Copper Nickel 30%, Spring
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-10 Aerospace Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-10 Industrial Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-10 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-12 Aerospace Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-11 Aerospace Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-11 Industrial Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-12 Industrial Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-20 Industrial Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-30 Industrial Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-40 Industrial Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-62 Industrial Woven Fabric 312
Information provided by 3M
Tensile Modulus 152 GPa
22000 ksi
Typical epoxy composite property
Hexcel® HexTow™ AS4D Carbon Fiber
HexTow™ AS4D carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized to improve ..
Tensile Modulus 152 GPa
22000 ksi
filament
3M Nextel™ AF-14 Industrial Woven Fabric 312
Information provided by 3M