Mechanical Properties Metric English Comments
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC
LNP* THERMOCOMP* DC006H is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC (Asia Pacific)
LNP* Thermocomp* DC006H is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT
LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead.
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT (Asia Pacific)
LNP* Thermocomp* WFB54 is a compound based on Polybutylene Terephalate resin containing Glass Bead.
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly
LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX95523C PC
LNP* STAT-KON* DX95523C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX95523C PC (Asia Pacific)
LNP* Stat-kon* DX95523C is a compound based on Polycarbonate resin. Added features of this material include: Electrically Conductive.
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific)
LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive.