Polymer Property : Tensile Modulus = 24.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 24.0 GPa
3480 ksi
Plastcom SLOVAMID 6 GF 60 000/1M PA6 reinforced with 60% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 60% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go..
Tensile Modulus 24.0 GPa
3480 ksi
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. ..
Tensile Modulus 24.0 GPa
3480 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural..
Tensile Modulus 24.0 GPa
3480 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
Tensile Modulus 24.0 GPa
3480 ksi
dry; ISO 527-1/-2
DSM Stanyl® TW200B6 PA46-CF30
30% Carbon Reinforced, Heat Stabilized, Lubricated
Tensile Modulus 24.0 GPa
3480 ksi
dry; ISO 527-1/-2
DSM Stanyl® TW271B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
Tensile Modulus 24.0 GPa
3480 ksi
dry; ISO 527-1/-2
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
Tensile Modulus 24.0 GPa
3480 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat..
Tensile Modulus 24.0 GPa
3480 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat..
Tensile Modulus 24.0 GPa
3480 ksi
ISO 527
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black
Information provided by Eurotec®
Tensile Modulus 24.0 GPa
3480 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66...
Tensile Modulus 24.0 GPa
3480 ksi
ISO 527
Eurotec® Tecopet® PT74 CR30 BK111 PR PET, 30% carbon fiber reinforced, black, fast crystallization grade
Information provided by Eurotec®
Tensile Modulus 24.0 GPa
3480 ksi
ASTM D638
Quantum Composites QC-8770 63% Glass Fiber Hybrid Vinyl Ester SMC  (discontinued **)
QC-8770 is a hybrid vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and excellent st..
Tensile Modulus 24.0 GPa
3480 ksi
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..