Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.0 GPa | 2470 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 CF 20 Polyamide 66, 20% Carbon Fiber FeaturesChemically reinforced with 20% carbon fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. .. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)
(Unverified Data**) Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA)
(Unverified Data**) Ixef 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance. - Natural: Ixef.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ASTM D638 |
Glastic BMC SLC-1000 Glass-Reinforced Polyester Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-1/-2 |
Lanxess Pocan® T 7391 000000 PBT + PET, 45% Glass Fiber PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanica.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Omnix® FC-9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® FC-9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ASTM D638 |
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-1/-2 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50 Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LV-65H FWA black 9225 is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40 Information provided by EMS Grivory |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 6.6 CF 20 Polyamide 6.6 carbon fiber This material has very high strength and a high operating temperature. It can be used for precision components, drive parts and housings.Information provided by CENTROPLAST Engineering Plastics GMB.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-1 |
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo.. |