Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM Data |
Americas Styrenics Styron® XL-8028 High Impact Polystyrene
(discontinued **) STYRON® XL-8028 high impact polystyrene is designed for VCR cassettes, toys, small appliances, telephones, housewares, tool items, computer consoles and bodies for computer cartridges. It offers hi.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
Ineos ABS Lustran® QE 1094 AS, Injection Grade
(discontinued **) Injection molding grade, super high impact.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
Ineos ABS Lustran® E401 Very high surface resistance, high surface gloss.,Property data per ISO test methods. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
|
LATI Latene® 11 MDT05-01 PP Homopolymer Polypropylene homopolymer (PPh) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
LATI Latimass 63-06 D025 PA66 Specific density compound based on Polyamide 66 (PA66). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Sol.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1mm/min; ISO 527 |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1mm/min, 4mm injection molded, unannealed; ISO 527-2 |
Styron EMERGEâ„¢ 5100 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5100 is a pre-colored, white, ABS resin, having high opacity and excellent toughness intended for manufacture of laser-marketable injection-molded smart cards.Information provided b.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL IN120 PPE+HIPS (Europe-Africa-Middle East) NORYL IN120 is an unfilled material with a Vicat B/120 of 125 °C according ISO 306. NORYL IN120 has been developed for the interior automotive |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527-1/-2 |
Unitika EX-1222 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | Film T.D.; ASTM D882 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | Film T.D.; ASTM D882 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | cond; ISO 527-1/-2 |
DSM Akulon® K224-PG2 PA6-I-GF8 8% Glass Reinforced, Impact Modified |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527-1/-2 |
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Eastman Eastar GN078 Copolyester, Natural Eastar Copolyester GN078 builds on the strength of Eastar Copolyester GN077 by offering improved melt strength and toughness. Eastar Copolyester GN078 does not meet FDA compliance but is an excellen.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min |
Arkema Group Orgalloy® LE 6006 Nylon Alloy, 6% Glass Fiber Reinforced (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).6% glass fiber reinforced. Medium stiffness, good thermomechanical.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers. |