Mechanical Properties Metric English Comments
Tensile Modulus 19.5 GPa
2830 ksi
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre
FeaturesPA 6/66 for injection moulding, chemically strengthened with 30% of carbon fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-..
Tensile Modulus 19.5 GPa
2830 ksi
ISO 527
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Tensile Modulus 19.5 GPa
2830 ksi
ISO 527
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
Tensile Modulus 19.5 GPa
2830 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Modulus 19.5 GPa
2830 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Modulus 19.5 GPa
2830 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Modulus 19.5 GPa
2830 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Modulus 19.5 GPa
2830 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Modulus 19.5 GPa
2830 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Modulus 19.5 GPa
2830 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive.
Tensile Modulus 19.5 GPa
2830 ksi
ASTM-D790
Polyram RamTough PZ301R8 Polycarbonate, 40% Carbon Fiber
40% Carbon fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Tensile Modulus 19.5 GPa
2830 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Tensile Modulus 19.5 GPa

@Temperature 23.0 °C
2830 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..