Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 20.0 GPa | 2900 ksi | ASTM D-638 |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ASTM D-638 |
PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Tensile Modulus | 20.0 GPa @Temperature 23.9 °C |
2900 ksi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ASTM D-638 |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | Conditioned; ISO 527-2 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1028 Polyarylamide (PARA)
(discontinued **) Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON AE006 ABS LNP* STAT-KON* AE006 is a compound based on ABS containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass Balanced fabric 300 g/m2 Information provided by HexCel |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-60 PA666-GF60 Product description: Grilon TSG-60 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers. Grilon TSG-60 has the following important properties: Very high st.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Eurotec® Tecomid® NA40 CR30 BK111 PA6.6, 30% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Eurotec® Tecomid® NBX0 GR60 NL PA6, 60% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Conditioned, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ASTM D638 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton OV00A PPS LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |