Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.00 GPa | 435 ksi | Type 1B, 50mm/min; ISO 527-1/2:1993 |
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass .. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Nilit FRIANYL B63 F Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, highly crystallized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B70 UF V2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Nilit FRIANYL B63 H Nylon 6 for injection molding Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 127UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 127UV BK701 is a high viscosity, UV stabilized acetal homopolymer. It has excellent impact strength, UV resistance and thermal stability. It is well suited for automotive interior applicati.. |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46 LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 218 Black 21 N PA66/6, DRY Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1mm/min; ISO 527-2/1A |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DSM Akulon® S227-C Nylon 66 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15 Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BM-30 PA6-MD30 Product description: Grilon BM-30 is a 30% mineral reinforced PA6 injection moulding grade. Grilon BM-30 has the following important properties: heat stabilizedimpact resistantisotropic shrinkagelig.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6 Information provided by EMS Grivory |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 500SC NC010 Acetal (POM)
(Unverified Data**) Silicone Lubricated Medium Viscosity Acetal Homopolymer Concentrate Developed for Enhancing LubricityInformation provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® F 47 NL nat 6028 PA6 Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1mm/min; ISO 527 |
BASF Ultramid® B50L 01 PA6 (Dry) Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM Test |
BASF Ultramid® B50L 01 PA6 (Dry) Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 1000-11 NF2001 PA66 (Dry) Ultramid 1000-11 NF2001 is a general purpose nylon 6/6. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® SC652 NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry Delrin SC652 is a medium viscosity acetal homopolymer with an advanced system of l.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® G 21 PA6I/6T Product description: Grivory G 21 natural 6506 is a high viscosity, partially aromatic, amorphous copolyamide with processing aid. Improved gas and aroma barrier at elevated relative humidityExcelle.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Polyram RamOfin PPC350M6 Polypropylene, 30% Mineral Filled 30% Mineral filled, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |