Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.07 GPa | 300 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | 0.2 inches/minute; ASTM D 638 |
NOVA Chemicals Dylark® FG2500 High-Heat Styrenic Copolymer Product Description and Features: Styrenic copolymer with high-heat resistance, high-impact strength and good toughness. Resins used in food grade sheet extrusion and injection molding application.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D 638 |
Styrolution PS 5801 HIPS Exceptional processabilityHigh toughnessUSP Class VI certifiedUl Classification 94 HBInformation provided by Styrolution |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM Data |
Styron Magnum™ 344HP ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | >= 2.07 GPa | >= 300 ksi | |
Master Bond EP21NDLO Low Outgassing, Room Temperature Curing Two Component Epoxy Master Bond EP21ND-LO is a two component, room temperature curing epoxy system for bonding, sealing and coating featuring outstanding physical properties. EP21ND-LO has a convenient one to one mix r.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
Westlake Plastics Ardel® Polyarylate Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
Total PSI 825E Polystyrene Polystyrene 825E is a high impact polystyrene designed specifically for extrusion/thermoforming. Over the years, this popular resin has established itself as the standard extrusion grade high impact.. |
|||
Tensile Modulus | 2.07 - 2.41 GPa @Temperature 23.9 °C |
300 - 350 ksi @Temperature 75.0 °F |
|
Master Bond EP21CLV Two Component Epoxy System Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
Ensinger Tecanat™ Unfilled Polycarbonate (PC) Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D412 |
Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
ExxonMobil Paxon™ AA50-002 Blow Molding Resin
(discontinued **) AA50-002 is a blow molding grade high density polyethylene. This resin has excellent stress crack resistance combined with high impact strength, rigidity, and melt strength.Information provided by .. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | blown films TD; ISO 527-3 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ AT-000/000 ESD Acetal-Copolymer
(discontinued **) Description/Features:AntistaticInformation provided by PolyOne Corporation. |