Mechanical Properties Metric English Comments
Tensile Modulus 320 GPa
46400 ksi
Young's; DINV ENV 843-2
CeramTec B 601 Alumina, 98.5%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Tensile Modulus 320 GPa
46400 ksi
Goodfellow TZM Molybdenum High Temperature Alloy
Increased high temperature strength over pure molybdenum although, like Molybdenum, it oxidizes rapidly in oxidizing atmospheres above 500°CInformation provided by Goodfellow.
Tensile Modulus 320 GPa
46400 ksi
Cytec Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..