Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527-2 |
Pasargad Polymer Peyvand Pasalen 3P-H3230B1 Polypropylene, 30% Mineral Filled Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 HI Polyamide 6, Impacted FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | |
Plastcom SLOVAMID 6 HI/1 TLS PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific) High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ASTM D638 |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® FXX210SK PBT+PC (Europe-Africa-Middle East) XENOY FXX210SK is an unreinforced PBT+PC injection moulding resin with excellent impact characteristics and containing a metal sparkle Visual FX. Applications: automotive bezels and appliances. XENO.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
Styron Pulse® 920 MG PC/ABS An inherently matt medium heat, medium impact PC/ABS resin, PULSE™ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527 |
Wico Plast Wicolon 407 Polycarbonate, U.V. Stabilized ApplicationsInjection moldingCharacteristics:U.V. stabilizedAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527-1/-2 |
Covestro Makrolon® 1248 Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Formerly Makrolon KU1-1248MVR (300 °C/1.2 kg) 7.0 cm3/10 minFood contact qualityMedium viscosityImpact modifiedInjection molding - Melt temperature 280 - 320 °CAvailable in.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527 |
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527 |
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural Information provided by Eurotec® |
|||
Tensile Modulus | >= 2.25 GPa @Temperature 20.0 °C |
>= 326 ksi @Temperature 68.0 °F |
Elasticity |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1mm/min; ISO 527 |
Teijin Multilon T-2711 Standard, Automobile Part Series PC/ABS Polymer Alloy PC/ABS polymer alloy general grade developed for automobile parts use. It has high heat resistance, impact strength, light resistance and fluidity, particularly, the high impact strength in a wide r.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min |
Polimeri Europa SINKRAL PD F332 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MGN,105-15-16-20 General purpose injection grade which combines excellent thermal stability during processing with.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min |
Polimeri Europa SINKRAL G323 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-20 General purpose injection moulding grade. Main properties are: good impact resistance high flow e.. |