Polymer Property : Tensile Modulus = 330 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Total 819E Polystyrene  (discontinued **)
Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof..
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
I. Stern HIPS 8 High Impact Polystyrene Injection Grade
Features:Good processing characteristicsComplies with FDA requirements as described in Title 21 CFR 177.1640ApplicationsDisplaysHouse waresStructural FoamInformation provided by I. Stern & Co. Inc.
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
LG Chemical Lupoy 1621-02 Polycarbonate Resin
Description: LUPOY PC 1621-02 resin is designed for large injection stretch blow molding and extrusion blow molding parts. It exhibits an excellent physical property balance of heat resistance, tran..
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Spartech Acrylloy 7 Acrylic Sheet
Description: Acrylic SheetInformation provided by Spartech.
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Spartech Acrylloy F Acrylic Sheet
Description: Acrylic SheetInformation provided by Spartech.
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Star Plastics ABS3030 Molding Grade ABS
Information provided by Star Plastics, Inc.
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Styron Pulse® 2000 ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Modulus 2.28 GPa
330 ksi
ASTM 638
Chase Plastics CP Pryme® PC100RHF Polycarbonate
Form: PelletsInformation provided by Chase Plastics.
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Modulus 2.28 GPa
330 ksi
ASTM D-638
Axiall UV-6685 Rigid PVC, Molding
Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation.Info..