Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.34 GPa | 339 ksi | 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | ASTM D638 |
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet) |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Asia Pacific) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD103 PC FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXD103R PC FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXM121R PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regi.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ HTX M6215 Polyvinyl Chloride Alloy (PVC Alloy) It is recommended that the compound pellets be dried for 3 to 4 hours at 150 deg. F.Information provided by PolyOne |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXD941A PC FXD153 is an Extrusion / Blow molding grade in a Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Co.. |
|||
Tensile Modulus | 2.34 GPa @Thickness 3.18 mm |
339 ksi @Thickness 0.125 in |
ASTM D638 |
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU) Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins... |
|||
Tensile Modulus | 2.34 GPa @Thickness 3.18 mm |
339 ksi @Thickness 0.125 in |
ASTM D638 |
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | ASTM Data |
Styron CALIBRE™ 300 15 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | ASTM Data |
Styron CALIBRE™ 300EP 22 Polycarbonate, General Purpose CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
Tensile Modulus | 2.34 GPa @Thickness 3.20 mm |
339 ksi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can .. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | Storage |
Epoxy Technology EPO-TEK® 375 High Temperature Epoxy Product Description: EPO-TEK®375 is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. Also available in a single component frozen sy.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |