Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 24.0 GPa | 3480 ksi | |
Plastcom SLOVAMID 6 GF 60 000/1M PA6 reinforced with 60% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 60% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | |
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**) Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural.. |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TW271B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat.. |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat.. |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | ISO 527 |
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66... |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | ISO 527 |
Eurotec® Tecopet® PT74 CR30 BK111 PR PET, 30% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | ASTM D638 |
Quantum Composites QC-8770 63% Glass Fiber Hybrid Vinyl Ester SMC
(discontinued **) QC-8770 is a hybrid vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and excellent st.. |
|||
Tensile Modulus | 24.0 GPa | 3480 ksi | |
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |