Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.69 GPa | 390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging VB9-51 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP J1000AE PES LNP* COLORCOMP* J1000AE is an unfilled Polyethersulfone. Added feature of this grade is: Easy Molding. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boi.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet) |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **)< Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM-D638 |
Ineos ABS Lustran® 427 |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Fiberfil® J-68/20/E/SD Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU) Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved .. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU) Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, .. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU) Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU) Veradel® 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam,.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU) Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Tensile Modulus | 2.69 GPa @Thickness 3.20 mm |
390 ksi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Videolar 535 Crystal Polystyrene (GPPS) Designed for injection molding, extrusion, and blow moldingVery easy flowing grade for general useExcellent processability for multiple cavity moldsFeatures: Excellent strengthGood temperature resis.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | |
Loctite® Output™ 315 Acrylic Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D-638 |
Axiall HF-6597 Rigid PVC, Molding Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provide.. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and .. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Tensile Modulus | 2.69 - 3.10 GPa | 390 - 450 ksi | ASTM D638 |
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView .. |
|||
Tensile Modulus | 2.69 GPa | 390 ksi | ASTM D638 |
Fiberfil® J-68/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |