Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.70 GPa | 392 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 6 BT B 27 PA6 Basic type PA 6 for compounding, for general use. Grade can contain PA 66 up to 5% and TiO2 content up to 0.25 %. Use: automotive, engineering, electrical and consumer-goods industryInformation Prov.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 6 BT N 32 B PA6 Basic type PA 6 for compounding, for general use. Delivered in the natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PC 51 T 20 Polypropylene Copolymer, 20% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 FRC 2 Polyamide 6, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electro-technical purposes. Excellent flow of the material predetermines.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY FXW750SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Med. Heat & Impact Resin |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | dry |
Ineos ABS Triax® KU2-3154 ABS + Nylon 6 Mineral reinforced, easy flowing, reduced moisture absorption, very low warpage, injection molding, pellets.,Property data per ISO test methods. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® C CF 407 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1, -2; 1 mm/min |
Lanxess Pocan® B 1701 000000 PBT PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS. |
|||
Tensile Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
1mm/min; ISO 527-2/1A/1 |
SYNTHOS Forsan® 393 Acrylonitrile Butadiene Styrene (ABS) High heat resistance, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Ka.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9500GW PET+PC (Europe-Africa-Middle East) Unfilled Flameretardant PET/PC blend for GWIT.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1mm/min; ISO 527 |
Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1 |
Sax Polymers SAXLAC 207 Acrylonitrile Butadiene Styrene Saxalac 207 is a high heat ABS, characterized by high impact strength and high stiffness.Mechanical property data tested at 50% RH.Information provided by SAX Polymers |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
Cyclics CBT® 100 Thermoplastic Resin CBT® 100 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
Cyclics CBT® 200 Thermoplastic Resin CBT® 200 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AF is a high viscosity acetal homopolymer containing 20% Teflon PTFE fibers. It is designed for a.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 909 WR POM Copolymer unreinforced, UV-stabilized POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-2 |
CENTROPLAST CENTRO HPM Polysulfone This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Informatio.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® C CE 407 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |