Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.12 GPa | 598 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4211 PC Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Modulus | 4.12 GPa | 598 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4211 PC (Asia Pacific) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Modulus | 4.12 GPa | 598 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 4.12 GPa | 598 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Modulus | 4.12 GPa | 598 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 4.12 GPa | 598 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Tensile Modulus | 4.12 GPa | 598 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Tensile Modulus | 4.12 GPa | 598 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Tensile Modulus | 4.12 GPa @Temperature 80.0 °C |
598 ksi @Temperature 176 °F |
ISO Data |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |