Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.20 GPa | 609 ksi | CD; DIN EN ISO 527 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-2/1A |
Radici Raditer® B RVA 100 Polybutylene Terephthalate with 10% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-1/-2 |
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data) Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Victrex® ST™ P45 PolyEtherKetoneEtherKetoneKetone (PEKEKK), High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, coarse powder for extrusion compounding, low flow, color natural.Information Provid.. |
|||
Tensile Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Nilit RECONYL A SG30 Recycled nylon 6.6 for injection molding, 30% mineral filled Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-2 |
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Europe-Africa-Middle East) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ASTM-D790 |
Polyram RamOfin PPC342M6 Polypropylene, 30% Mineral Filled 30% mineral filled, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP 7665 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD20(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledPreprocessingMax. Water content |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 50mm/min; ISO 527-1 |
Denka CL-430 Transparent Resin Polymer (MABS) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Tensile Modulus | 4.20 GPa @Temperature 120 °C |
609 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |