Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.29 GPa | 622 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 4.29 GPa | 622 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific) LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |