Polymer Property : Tensile Modulus = 409 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.82 GPa
409 ksi
MD; ASTM D638
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
Tensile Modulus 2.82 GPa
409 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Dry Blend E1354 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.82 GPa
409 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC
LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.82 GPa
409 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific)
LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.82 GPa
409 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DD0009 PC
LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Tensile Modulus 2.82 GPa
409 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Tensile Modulus 2.82 GPa
409 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Tensile Modulus 2.82 GPa
409 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC (Asia Pacific)
LNP* Stat-kon* DD0009XP is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include:Electrically Conductive, Flame Retardant. Also known as Stat-Kon*..
Tensile Modulus 2.82 GPa
409 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 310SE0 PBT
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Tensile Modulus 2.82 GPa
409 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Tensile Modulus 2.82 GPa
409 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC
LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.