Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87564 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/20T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific) LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Nilit Polynil® P50FI Internally Lubricated Nylon 66 Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/5T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU) Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product .. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY SLDM2005 PC (Asia Pacific) Antistatic Polycarbonate, Non Halogen FR V-2 grade, mineral 5% filled |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Westlake Plastics Pomalux® Acetal Copolymer Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Ensinger Tecatron® XP-72 Compression Molded PPS Compound, 20% PTFE Filled Natural Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Ensinger PVC Polyvinylchloride (PVC) Ensinger's type 1 grey PVC ROD is designed for machining solutions and is a cost effective solution for general industrial applications. The material offers an excellent combination of chemical resi.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall HR-5009 Rigid PVC, Molding Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which incl.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall NR-5009 Rigid PVC, Molding Georgia Gulf NR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent processability, .. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall 2502 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall 2506 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall 8266 Natural 02 Rigid PVC, Extrusion, Natural 02 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall 2503 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |