Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet) Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | |
Ineos ABS Lustran® SAN 31 51 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | |
Hexcel® HexPly® EH04 Epoxy Resin System HexPly® EH04 is a modified epoxy resin system specifically designed for bladder molding or sheet wrap tube applications. Unique chemistry provides full cured parts in only 3 minutes at 138°C.Appli.. |
|||
Tensile Modulus | >= 3.45 GPa | >= 500 ksi | |
Master Bond EP42HT-2AO-1 Two Part, Cryogenically Serviceable Epoxy Description: Master Bond EP42HT-2AO-1 Black is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material that meets NASA low outgassing specifications. It featu.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D822 |
DuPont Teijin Films Mylar® CL Polyester Film, 50 Gauge Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM Data |
Dow Tyril® 880B SAN TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.Data provided b.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® UR-20CF/000 Thermoplastic Elastomer - TPU, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |