Polymer Property : Tensile Modulus = 598 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 4.12 GPa
598 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HFD4211 PC
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Tensile Modulus 4.12 GPa
598 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HFD4211 PC (Asia Pacific)
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Tensile Modulus 4.12 GPa
598 ksi
5.1 mm/min; ASTM D638
PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Tensile Modulus 4.12 GPa
598 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East)
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Tensile Modulus 4.12 GPa
598 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC
LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated.
Tensile Modulus 4.12 GPa
598 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 7062HP PBT
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Tensile Modulus 4.12 GPa
598 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Tensile Modulus 4.12 GPa
598 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Tensile Modulus 4.12 GPa

@Temperature 80.0 °C
598 ksi

@Temperature 176 °F
ISO Data
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET
Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in..