Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0420 GPa | 6.09 ksi | 1 mm/min |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 0.0420 GPa | 6.09 ksi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |