Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.20 GPa | 609 ksi | MD; DIN EN ISO 527 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | CD; DIN EN ISO 527 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Nilit FRIANYL B63 KF20 Nylon 6 for injection molding, 20% short glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.20 GPa @Thickness 0.100 mm |
609 ksi @Thickness 0.00394 in |
TD; ISO 527 |
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Victrex® ST™ P45 PolyEtherKetoneEtherKetoneKetone (PEKEKK), High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, coarse powder for extrusion compounding, low flow, color natural.Information Provid.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Nilit RECONYL A SG30 Recycled nylon 6.6 for injection molding, 30% mineral filled Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-2 |
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Tensile Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Grupo Repol Dinalon® A1X25 V0 PA66, V0 red phosphorus and halogen free Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AF0029 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp WB006 PBT LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD20(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledPreprocessingMax. Water content |
|||
Tensile Modulus | 4.20 GPa @Temperature 180 °C |
609 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® OCD2100 BK27021 PA46-GF40 40% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
Eurostar Starpylen MZ006S PP, Glass Fiber Filled, Injection Molded Starpylen MZ006S is a Glass fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WT 30GF S3)Information provided by Eurostar. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | Transverse direction; ISO 527/4 |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Conditioned, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 4.20 GPa @Temperature 120 °C |
609 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |