Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 62.1 GPa @Temperature 23.9 °C |
9000 ksi @Temperature 75.0 °F |
0° Direction, Dry; Oven Cure 250°F, 90 min; ASTM D3039 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Tensile Modulus | 62.1 GPa | 9010 ksi | ASTM D638 |
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9593 (127-51-5) is a 3K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics.. |
|||
Tensile Modulus | 62.1 GPa @Temperature 73.0 °C |
9000 ksi @Temperature 163 °F |
Laminate property; Dry |
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |