Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.20 GPa | 1040 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6 GF 20 FRA 5 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 20% glass fiber, flame retarded with halogen flame retardant. Main features: flammability in accordance with UL 94 5 at 1.6 mm, glow wire at 960°C. Appli.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527 |
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Radici Radilon® S RV200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Radici Radilon® S RV300R (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Radici Radilon® S RV330 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-2/1A |
Radici Raditer® B RV 200 Polybutylene Terephthalate with 20% Glass fiber Raditer® B RV 200 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Tensile Modulus | 7.20 GPa @Temperature 23.0 °C |
1040 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 49 GF 30 003/3M Polypropylene reinforced with glass fiber, heat stabilized Modified homopolymer PP for injection molding, reinforced with 30% glass fiber, heat stabilized. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 7.20 GPa @Temperature 23.0 °C |
1040 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK642FR BK851 PBT
(Unverified Data**) Crastin® SK642FR BK851 is a black 15% glass fiber reinforced, flame retardant polybutylene terephthalate for injection molding. It has a UL94 V-0 rating @ 0.75mm.Information provided by DuPont Perf.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527 |
Grupo Repol Dinalon® B1S25 M404 PA6 40% Mineral Charge Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
DSM Akulon® F249-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK642FR BK851 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR BK851 is a black 15% glass fiber reinforced flame retardant polybutylene terephthalate for injection molding. It has a.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20 Product description: Grivory GV-2 FWA black 9225 is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copoly.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |