Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 7.80 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 7.80 GPa
1130 ksi
ISO 527-2
PolyOne Nymax™ GMF 604 40 UV Black 115 1 X 1 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
Tensile Modulus 7.80 GPa
1130 ksi
Plastcom SLOVAMID 66 GB 30 GF 20 PA66, 20% glass fibre, 30% glass beads
FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 30 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b..
Tensile Modulus 7.80 GPa
1130 ksi
STN EN ISO 527-2
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber
FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
Tensile Modulus >= 7.80 GPa
>= 1130 ksi
ISO 527-1,2
Qualchem Danamid AFGFS2HUV30 Polyamide 66, 30% Glass Fiber
Reinforced with glass fiber. Impact modified, heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial lights.Information provided by Qualchem Zrt.
Tensile Modulus 7.80 GPa

@Thickness 4.00 mm,
Temperature 23.0 °C
1130 ksi

@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/1
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Tensile Modulus 7.80 GPa

@Temperature 23.0 °C
1130 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT  (Unverified Data**)
Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta..
Tensile Modulus 7.80 GPa
1130 ksi
cond.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Tensile Modulus 7.80 GPa
1130 ksi
LATI Latilub 82-05GR G/30 PA12, 30% Glass Fiber Reinforced, Graphite Filled
Self-lubricating product based on Polyamide 12 (PA12). Graphite. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Modulus 7.80 GPa
1130 ksi
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant
Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Tensile Modulus 7.80 GPa
1130 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON RX98063 PA 66 (Europe-Africa-Middle East)
LNP* STAT-KON* RX98063 is a compound based on PA 66 resin containing Glass Fiber, Stainless Steel Fiber. Added features include; Antistatic.
Tensile Modulus 7.80 GPa
1130 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC
LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare.
Tensile Modulus 7.80 GPa
1130 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66
LNP* STAT-KON* RE002 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 7.80 GPa
1130 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific)
LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 7.80 GPa
1130 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP NF0061 PC+ABS (Europe-Africa-Middle East)
LNP* THERMOCOMP* NF0061 is a compound based on PC+ABS resin containing Glass Fiber, Flame Retardant. Added features include : Flame Retardant.
Tensile Modulus 7.80 GPa
1130 ksi
ASTM D638
Plenco 7100 Phenolic, Nodular, Injection Molded
PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit..
Tensile Modulus 7.80 GPa
1130 ksi
ISO 527
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers
Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch..
Tensile Modulus 7.80 GPa
1130 ksi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..
Tensile Modulus 7.80 GPa
1130 ksi
ASTM D638
Plenco 2300 Phenolic, Granular, Transfer Molded
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654..
Tensile Modulus 7.80 GPa
1130 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® LV-3 ESD PA12-GF30
Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where..
Tensile Modulus 7.80 GPa
1130 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30
Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010..
Tensile Modulus 7.80 GPa
1130 ksi
ISO 527-1/-2
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR BK851 is a 20% glass fiber reinforced flame retardant black polybutylene tere..
Tensile Modulus 7.80 GPa
1130 ksi
ASTM D638
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Tensile Modulus 7.80 GPa
1130 ksi
ISO 527-1
Barlog Plastics KEBATER BFA20 PBT, 20% glass fiber reinforced, flame retardant
PBT-GF20 FRInformation provided by BARLOG plastics GmbH.
Tensile Modulus 7.80 GPa
1130 ksi
1 mm/min
Arkema Group Rilsan® BZM 30 TL Nylon 11, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MHL,18-050,GF30Rigid grade with glass fiber (30%) filler for injection molding. Available colors: black and natural. Light and heat stabilized.Rigidity. High compressive st..
Tensile Modulus 7.80 GPa
1130 ksi
1mm/min; ISO 527
Teijin Panlite® BS-8110R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin
CF 10% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact..
Tensile Modulus 7.80 GPa
1130 ksi
ASTM D638
Plenco 2000 Phenolic, Granular, Transfer Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..
Tensile Modulus 7.80 GPa
1130 ksi
ISO 527-1/-2
Suzhou Hipro Polymers Hiprolon® 90 MC HLS G30 Nylon 612, 30% glass fiber filled
Hiprolon® 90 MC HLS G30 is a polyamide 6.12 compound reinforced with 30% chopped glass fiber, and is used for injection molding. Features: high dimension stability, chemical resistance, impact resi..
Copyright © lookpolymers.com All Rights Reserved