Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.93 GPa | 1150 ksi | ASTM D638 |
Techmer ES Electrafil® J-3/CF/10 Nylon 6, 10% Carbon Fiber Reinforced |
|||
Tensile Modulus | 7.93 GPa | 1150 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66 LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |