Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.83 GPa | 700 ksi | TM R050-36 |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Tensile Modulus | 4.83 GPa | 700 ksi | TM R050-36 |
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Tensile Modulus | 4.83 GPa | 700 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PS-15GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 4.83 GPa | 700 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PK-15GP/5T Polyetheretherketone (PEEK), PTFE Lubricated
(discontinued **) Description/Features:Graphite LubricatedPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 4.83 GPa | 700 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-15GF/10T Acetal-Copolymer, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 4.83 GPa | 700 ksi | ASTM D638 |
Ensinger Tecapeek® XP-115 Compression Molded PEEK Compound, Static Dissipative Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 4.83 GPa | 700 ksi | ASTM D-638 |
Axiall Tuf-Stif 2802 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2802 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
Tensile Modulus | 4.83 GPa | 700 ksi | ASTM D638 |
Asahi Kasei Thermylene® P-30FG-0812 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Modulus | 4.83 GPa | 700 ksi | ASTM D638 |
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |