Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.40 GPa | 1220 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP6GF43 Nylon 6, 43% Glass Reinforced, Dry Nylon 6 - Glass reinforced (43 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527-1/2 |
Radici Radilon® SERV3808 K (dry) Nylon 6 Heat stabilized glass-fiber reinforced with high impact strengthInformation provided by Radici group. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 |
Radici Radilon® WIT 30/28 Nylon 66-GF30 Automotive cooling liquid resistant PA66-GF30 grade designed to be processed by WIT technology.Information provided by Radici group. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features include; Internally Lubricated, Easy Molding. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 |
Nilit FRIANYL B63 FK 2010 Nylon 6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 25 H2.0 LT 904040 Nylon 6, 25% Glass Fiber PA 6, injection molding grade, 25% glass fibers, good heat-ageing resistance, laser-weldable |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527-1/-2 |
Lanxess Pocan® KL 1-7033 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, impact modified |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | |
LATI Latiohm 90/13-09 PD01 G/10 PPOm, 10% Glass Fiber Reinforced Semiconductive/dissipative product based on Modified Polyphenylene Oxide (PPOm). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA6.10 (Europe-Africa-Middle East) LNP*Lubricomp* QFL36 is a compound based on PA 6/10 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 Type 1A |
Solvay TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY Description: TECHNYL® AR 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled materials. This product is available in black .. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ASTM D638 |
Plenco 2408 Phenolic, Granular, Injection Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ASTM D638 |
Plenco 4301 Phenolic, Granular, Injection Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR BK099 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR BK099 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL BK039B is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF25 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ASTM D638 |
Plenco 7591 Phenolic, Pellet, Transfer Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |