Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.83 GPa | 1280 ksi | ASTM D638 |
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific) LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | ASTM D638 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 BK223 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | ASTM D638 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 NAT PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton MV00ASUV_WH9D703 PP Preliminary data for 50% Long fiber single color pellet filled PPThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
Tensile Modulus | 8.83 GPa | 1280 ksi | ASTM Test |
BASF Ultramid® B3WG6 BK00564 BGVW 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 BGVW is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |