Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.84 GPa | 1280 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® K4560 PBT 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Tensile Modulus | 8.84 GPa | 1280 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East) 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Tensile Modulus | 8.84 GPa | 1280 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DX13354 PC COPOLYMER (Asia Pacific) DX13354 is 30% glass fiber reinforced, impact modified and LDS functionalized polycarbonate resin. The features include LDS function, high flow, and good ductility. |
|||
Tensile Modulus | 8.84 GPa | 1280 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP OF008G PPS - LINEAR LNP* THERMOCOMP* OF008G is a compound based on PPS - Linear containing 15% Glass Fiber, 25% Milled Glass. |
|||
Tensile Modulus | 8.84 GPa | 1280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PX92248 PA 6 LNP* THERMOCOMP* PX92248 is a compound based on Nylon 6 resin containing Proprietary Filler(s). |