Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.80 GPa | 841 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 T 40 Polyamide 66, 40% Mineral Filled FeaturesPA 66 with the content of 40% chemically modified mineral filling. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cov.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CM4219 PC+ABS (Asia Pacific) |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | |
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre and 20% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, at 50% RH
(disc AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled
(Unve Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527, ASTM D638 |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
Nilit FRIANYL B63 W-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ASTM D638 |
North Wood Plastics PS with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Tensile Modulus | 5.80 GPa @Temperature 23.0 °C |
841 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 815UX PBT (Europe-Africa-Middle East) VALOX 815UX is a 15% glass reinforced PBT+PET blend with improved surface appearance and excellent UV performance. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PK0049 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0049 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Europe-Africa-Middle East) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527-1/-2 |
Covestro Makrolon® GF8001* Polycarbonate, 20% Glass Filled ISO 7391-PC,MR,(,,)-18-3,GF20Developmental productFormerly Makrolon DP1-1951MVR (300 °C/1.2 kg) 16 cm3/10 min20 % Glass fiber reinforcedLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1013GH15 1 NA/BK37 PA6-GF15 15% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-23H PA12-GF23 Product description: Grilamid LV-23H is a 23% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile. Good chemical resistanceGood UV stabili.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C140 BK086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding. It has very low warpage.Information provided by Du.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PK0049 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0049 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |