Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.00 GPa | 870 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nima™ HL 30530 GF FR PET, 30% Glass Fiber PET – Flame Retardant 30% Short Glass Fiber Reinforced. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM s.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP6GF50 Nylon 6, 50% Glass Reinforced, Conditioned Nylon 6 - Glass reinforced (50 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific) Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS.
Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Nilit FRIANYL A63 SG-GV 2010 Nylon 6.6 for injection molding, 20% mineral filled and 10% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Nilit FRIANYL A63 H-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)
(Unverified Data**) Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ASTM D638 |
Loxim 220 01HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
Lanxess Pocan® TP 740-101 000000 PBT + ASA, 15% Glass Fiber PBT+ASA, 15% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | |
LATI Latilub 66-01M G/15 PA66, 15% Glass Fiber Reinforced, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East) VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Polyram RamOfin PPH301G6NT Polypropylene, 30% Glass Fiber 30% Glass fiber reinforced polypropylene for injection molding applications. Approved and listed by WRAS Potable Water.Information provided by Polyram. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2VZ-15H PA6T/66-GF15 Information provided by EMS Grivory |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FE270046 BK267 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66 + Polyamide 6T/XTInformation provided by DuPont Performance Polymers |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR15 NL TD 28 PBT 15% glass fiber reinforced, UL94 V0, impact modified, high CTI Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Eurotec® Tecomid® NB30 GR13 BK EF PA6, 13% glass fiber reinforced, black, suitable for electrostatic powder coating Information provided by Eurotec® |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | dry; ISO 527-1/-2 |
DSM Akulon® K224-G3-FC NA99001 PA6-GF15 15% Glass Reinforced |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG3 (Dry) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-HXGM24 PA410-(GF+MD)30 % Glass Reinforced, % Mineral Reinforced, Heat Stabilized |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1 |
Barlog Plastics KEBATER BF115 PBT, 15% glass fiber reinforced PBT-GF15Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Conditioned, 25% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 12 GF 30 Polyamide 12 30% glass fiber CENTROMID 12 GF 30 is a dimensionally stable and high strength material with good electrical insulating properties. Its applications include levers and valve parts.Information provided by CENTROPLA.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Akulon® K220-HGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond)
(discontinu The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |