Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.20 GPa | 899 ksi | ASTM D638 |
PolyOne Edgetek® MLS-195A Polysulfone Alloy - ESD Material
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Conditioned, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG20-DN00N1 Nylon 6 20% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, DRY Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RB00A PA 66 (Europe-Africa-Middle East) 50% glass beads filled Polyamide 66 injection moulding resin. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS (Asia Pacific) LNP* Thermocomp* AF004L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP ZF004 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004 is a compound based on PPE+PS Blend resin containing Glass Fiber. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30 Information provided by EMS Grivory |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30 Information provided by EMS Grivory |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR430A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR430A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0069 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding Resin (also known as Starflam PA6 30E6 Z88)Information provided by Eurostar. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | ISO 527 |
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP KUR 1060 GFC Polypropylene, 30% Glass Filled PP copolymer 30% chemically coupled glass fiberElastomer modified, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Conditioned, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | ASTM D638 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PK0069 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0069 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |