Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 94.5 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 94.5 GPa
13700 ksi
ASTM D638
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC
AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc..
Tensile Modulus 94.5 GPa
13700 ksi
PSM Industries Pacific Sintered Metals Invar FN-251-S Powdered Metal
Coefficient of thermal expansion equal to glassInformation Provided by Pacific Sintered Metals, a division of PSM Industries
Copyright © lookpolymers.com All Rights Reserved