Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0951 GPa | 13.8 ksi | Plate Shear, L Direction, typical value |
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 3.5 Aramid Honeycomb Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod.. |
|||
Shear Modulus | 0.0950 GPa | 13.8 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |