Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.379 GPa | 55.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-327 - 3/16 - 8.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Modulus | 0.379 GPa | 55.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 3/8-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.379 GPa | 55.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.0025 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Modulus | 0.379 GPa | 55.0 ksi | silicone property; ASTM D1002 |
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |