Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 F is recommended for the .. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good clarity with LDPE.Applications: General purpose packaging, liners.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527 |
Total Finathene® LL 4010 FH 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 1184 |
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman E6838-902F Polyethylene Film
(discontinued **) Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business .. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman 1830F Polyethylene
(discontinued **) Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman D4004-F Polyethylene
(discontinued **) Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman D4028-F Polyethylene
(discontinued **) D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman E6838-969F Polyethylene
(discontinued **) E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap... |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882-02 |
Ipiranga Petrochem LB 0120 BP LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene LDPE 2100TN00: Heavy duty film suitable for application in shrink hoods, industrial sacks, heavy duty carrier bags and liners.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene LDPE 2102TX00 GP filmIt is used in wide range of widths and thicknesses e.g. for punches, bags, liners and lamination film.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527 |
Iran Petrochemical (PCC) LS0085 Low Density Polyethylene LS0085 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: thin shrink film.Information provided.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene LDPE 2004TC37: Light duty film used for very thin films requiring good optical properties for general packaging.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527-3 |
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Sclair® 11G1 LLDPE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionAdditives: Process stabilizer, Polymer process aidFilm properties are typical of blown film.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolym.. |