Polymer Property : Elmendorf Tear Strength, TD = 17.7 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD >= 17.7 g/micron
>= 450 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922
ExxonMobil Exceed™ 1518CA Tough Premium Film Resin  (discontinued **)
Exceed 1518CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518CA resin have outstanding tensile, impact strength and puncture. These superi..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922A
LyondellBasell Montell 16501F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922A
LyondellBasell Montell 16501F4 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922A
LyondellBasell Montell 16501F6 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets ..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922A
LyondellBasell Montell 16501F7 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922A
LyondellBasell Montell 16501F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin
Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation ..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922
Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922
Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin
Resin Type: Medium molecular weight distributionCharacteristics: Combination of toughness and tensileGood puncture resistanceMeets FDA regulations for food packaging below cooking temperaturesInform..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D882
Dow DAF 780 Carpet Underlayment Adhesion Film
DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D882
Dow INTEGRAL™ 925 High Heat Multilayer Adhesive Film
INTEGRAL 925 High Heat Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, fiberglass, non-wovens,..
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
Notched; ASTM D1992
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b..