Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 16.3 g/micron
413 g/mil
ASTM D1922
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 3 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b..
Elmendorf Tear Strength, TD 16.3 g/micron
413 g/mil
ASTM D1922
Dow DOWLEX™ 2038 Linear Low Density Polyethylene
Linear Low Density PolyethyleneInformation provided by Dow
Elmendorf Tear Strength, TD 16.3 g/micron
413 g/mil
ASTM D1922
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene
Fast processing on narrow die gaps For blown film paper product over wrap applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow