Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 52.0 g | 0.115 lb | Method A; ASTM D1709 |
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |