Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 100 g | 0.221 lb | F50; ISO 7765-1 |
Polimeri Europa Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexi.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ISO 7765-1 |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
Dart Drop Test | >= 100 g | >= 0.221 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4117N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | >= 100 g | >= 0.221 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | >= 100 g | >= 0.221 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ISO 7765-1 |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Formosa Plastics Formolene® L62608PE Film (Hexene Grade) LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D 1709/A |
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Dart Drop Test | 100 g | 0.221 lb | |
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Dart Drop Test | 100 g | 0.221 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA951000 Low Density Polyethylene ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene LF0200 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. LF0200 contains antioxidant.Applications: genera.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Westlake EF796 Low Density Polyethylene Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Westlake EF923 Low Density Polyethylene Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose.. |
|||
Dart Drop Test | >= 100 g | >= 0.221 lb | 40µm; ASTM D 1709 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Formosa Plastics Formolene® L62608 Film (Hexene Grade) LLDPE Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Dart Drop Test | 100 g @Thickness 0.0254 mm |
0.221 lb @Thickness 0.00100 in |
High Stalk Extrusion - 6:1 FLH/D ratio and 4:1 BUR; ASTM D1709A |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Film; 50.8 microns; ASTM D1709B |
Dow DX5E66 Polypropylene Homopolymer Resin OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil Escorene™ LD 708.62 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 708.62 is a 14.9% VA copolymer film resin. Film made from LD 708.62 exhibits good impact strength and superior heat sealabilty.Availability: Latin America, Nor.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM-D1709 |
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer FL31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processing .. |
|||
Dart Drop Test | 100 g | 0.221 lb | g/F50; ASTM D1709 |
Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Line.. |
|||
Dart Drop Test | 100 g | 0.221 lb | g/F50; ASTM D1709 |
Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene Liners, LDPE and HDPE blends; General use packages; Technical films for automatic packaging.Additives: Antiblock, DInformation provided by Braskem. |
|||
Dart Drop Test | 100 g | 0.221 lb | |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |