Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 55.0 g | 0.121 lb | F50; ISO 7765-1 |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
Dart Drop Test | 55.0 g | 0.121 lb | ASTM D1709 |
LG Chemical SEETEC BF415 LDPE Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Dart Drop Test | 55.0 g | 0.121 lb | Method A; ASTM D1709 |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |