Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709/A |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex FF 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FF 50.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | 25µ; ISO 7765-1 |
Total Finathene® LL 4010 FH 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Huntsman Rexell® M3104 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliant.Features: Excellent combination of toughness, stiffness, and optics with good temperature resistance.Applications: Diaper film.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Iran Petrochemical (PCC) Arak 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil LD 146.NH Packaging Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Huntsman PE1031 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
LyondellBasell Montell 16502F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
LyondellBasell Montell 16502F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA143063 Low Density Polyethylene ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA336149 Low Density Polyethylene ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ASTM D1709 A |
Equate EFDC-7050 LLDPE Film Extrusion Resin EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem F7018 LDPE Injection Molding Polyethylene F7018 is a low-density polyethylene with excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating, injection molding .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem FG31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FG31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blow film extrusion in blends with polyethylene. It has excellent mechanical propert.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FM31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blown film extrusion. It has excellent mechanical properties, especially hot tack. I.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D-1709A |
Bapolene® 122B Polyethylene, Film Grade Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. These.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Huntsman PE1158 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |