Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 138 MPa | 20000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 3381 Polyester Film Melinex® 3381 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well a.. |
|||
Film Tensile Strength at Break, TD | 138 MPa | 20000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 565 Polyester Film Melinex® 565 is a high clarity film which is differentially coated. One surface is coated with the standard T-Sub adhesion promoter; the opposite surface is coated for antistatic protection.Informa.. |
|||
Film Tensile Strength at Break, TD | 138 MPa | 20000 psi | ASTM D882 |
Dow Saran® 18L Clear Plastic Barrier Film Saran™ 18L is a clear biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow |
|||
Film Tensile Strength at Break, TD | 138 MPa | 20000 psi | ASTM D882 |
Honeywell MAP-Shield™ AF Generation 2 Shrinkable Barrier Film
(discontinued **) Description: MAP-Shield™ AF shrinkable barrier film is ideal for modified atmosphere packaged (MAP) food products in barrier trays for extended shelf life protection. The coextruded, biaxially orie.. |
|||
Film Tensile Strength at Break, TD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil OPPalyte® 310 HSTW OPP Film Product Description: One-side coated, white opaque OPP film with a proprietary cavitated core. It is designed for use unsupported or in a lamination for cold seal packaging applications. One side is.. |