Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 1000 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 1400 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 142 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 200 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 300 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 380 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 500 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 700 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 75 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 820 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329 Polyester Film, 92 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329S Polyester Film, 92 Gauge
An opaque white film with good handling properties, a unique glossy appearance, and a lower shrinkage for special applicationsInformation provided by DuPont.
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 329W Polyester Film, 300 Gauge
An opaque white film with good handling properties and a unique glossy appearance. 329W has same properties as 329 with the only exception being it is wound reverse. See the 329 datasheet for detail..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 339 Polyester Film, 1000 Gauge
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 339 Polyester Film, 300 Gauge
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 33..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 339 Polyester Film, 380 Gauge
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 339 Polyester Film, 700 Gauge
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 339 Polyester Film, 820 Gauge
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST339 Polyester Film, 1000 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST339 Polyester Film, 200 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST339 Polyester Film, 300 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST339 Polyester Film, 380 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST339 Polyester Film, 500 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST339 Polyester Film, 700 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 339 Polyester Film, 500 Gauge
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge
Melinex® 487 is a high-yield, white film that is coated on one side for adhesion to inks, coatings, laser printing, and thermal transfer printing.Information provided by DuPont.
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Mylar® MLB Polyester Film, 300 Gauge
Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML..
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339..