Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, TD = 20000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 138 MPa
20000 psi
ASTM D882A
DuPont Teijin Films Melinex® 3381 Polyester Film
Melinex® 3381 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well a..
Film Tensile Strength at Break, TD 138 MPa
20000 psi
ASTM D882A
DuPont Teijin Films Melinex® 565 Polyester Film
Melinex® 565 is a high clarity film which is differentially coated. One surface is coated with the standard T-Sub adhesion promoter; the opposite surface is coated for antistatic protection.Informa..
Film Tensile Strength at Break, TD 138 MPa
20000 psi
ASTM D882
Dow Saran® 18L Clear Plastic Barrier Film
Saran™ 18L is a clear biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow
Film Tensile Strength at Break, TD 138 MPa
20000 psi
ASTM D882
Honeywell MAP-Shield™ AF Generation 2 Shrinkable Barrier Film  (discontinued **)
Description: MAP-Shield™ AF shrinkable barrier film is ideal for modified atmosphere packaged (MAP) food products in barrier trays for extended shelf life protection. The coextruded, biaxially orie..
Film Tensile Strength at Break, TD 138 MPa
20000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil OPPalyte® 310 HSTW OPP Film
Product Description: One-side coated, white opaque OPP film with a proprietary cavitated core. It is designed for use unsupported or in a lamination for cold seal packaging applications. One side is..
Copyright © lookpolymers.com All Rights Reserved